Preparing to drill holes!
- DescriptionBefore you start to drill any holes in your new project you 'must' do the following. 
 Completely measure the thickness of the metal, spacing between the stones, measure the depth from the 'Table facet ' to the 'Culet'.
 If these are not taken into serious consideration, your project will encounter tough setting problems.
- AuthorGerry LewyWith over 40 years experience as a stone setter, Gerry Lewy is known throughout the diamond setting community. Gerry started his 9-year apprenticeship with a jewelry manufacturer and tutored by a gentleman ‘setter’, in Haddon Gardens, London. Gerry has redeveloped himself into more than a master setter, his purpose is now to be a teacher of the art as well. 
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.