The Hard Facts of Sapphires and Rubies
Ask any jeweler to list the gemstones with which they prefer to work, and sapphires and rubies would undoubtedly rank...
Read More
Hammering and Forging Safety Guidelines
Goldsmiths and silversmiths use hammers frequently in their work, silversmiths especially. A regular trade goldsmith might use a bench hammer...
Read More
Important Principles of Casting Safety
Here's something to aim for: a well laid-out, orderly workshop, well-lit by multiple non glare light sources, well-maintained equipment, electrically...
Read More
Pickling Notes
Jewelers treat soldered objects with dilute acid solutions to remove oxides produced from heating and soldering as well as glassy...
Read More
Patination Safety Considerations
Jewelers use so-called -oxidising- solutions to darken metals like silver, copper, brass, nickel silver, bronze and, with specialized mixtures, on...
Read More
Cracks in Jewelry Manufacturing
As many jewelry manufacturers and goldsmiths know from hard experience, cracking in jewelry can occur at any time during its...
Read More
Technology’s Relevance to Jewellery Design
Jewellery design is generally considered solely from an artistic standpoint, and the jewellery is viewed as an expression of a...
Read More
Jewelry Workshop Safety Report
This talk briefly reviews issues of studio safety and discusses ways of recognizing risks in the studio and reducing hazard...
Read More
Sample Consignment Agreement Contract
The following is Consignment Agreement contract. It is intended for information purposes only although if you wish to use it...
Read More
Solder Flow Retardant Notes
While goldsmiths normally strive to have their solder flow easily, there are times you don't want it to flow, such...
Read More
Depletion Gilding Notes
This is an academic paper, not a technical 'how to' guide. Many of the procedures described are unsafe in practice....
Read More
CNC Milling vs. 3D Printing
For someone new to the jewelry industry, the sheer assortment of tools and equipment in the typical workshop can be...
Read More
Notes on Presto-Lite Torch
We use a method for cutting down firescale when using a Presto-Lite Torch along with an acetylene B tank. The...
Read More
Learning Metalsmithing Process
An art school is in some ways a difficult place to learn to be a metalsmith. Traditional systems of industry...
Read More
Maintaining Good Workshop Air Quality
Four areas in the jeweler's workshop produce harmful substances that MUST be properly removed from the shop in order to...
Read More
Basic Fire Safety for Jewelers
Have a fire plan; ask your fire department for advice. Keep the appropriate extinguishers around and in good shape. Get...
Read More
The Effects of Global Warming on Pearl Oysters
Warming waters, changes in weather patterns, and increases in storm activity may all affect the future success of pearl farms,...
Read More
What Causes Casting Marks?
In the Spring 2003 Issue we asked the question "What causes these marks on this casting?" Around 100 readers responded...
Read More
Production Project Proposal
This is an example of a production project proposal involving the reproduction of two historically important buttons. This shows how...
Read More
Basic Chemical Storage Principles
There are a number of basic principles in storing chemicals. Know what your chemicals are, what their hazards are, their....
Read More
Art vs Craft
The Art versus Craft issue is a complex question and one that has bedeviled creators a great deal in the...
Read More
Studio Lighting Considerations
How you light your shop, illuminate your working area, experience the reflection from surfaces and the paint you choose for...
Read More
The Enamelist’s Vocabulary
Each medium has its own vocabulary and so it is with enamels and enameling. The glass glaze material that is...
Read More
Anodizing Principles Update
Although the basic anodizing principles involved in the reactive metals have been discussed in the past, a deeper insight into...
Read More
Craftsmanship Improvement Method
This is a method to reduce technical problems which one repeatedly experiences. We all find during the learning process that...
Read More
Safer Pickle Alternative
Procrastination can sometimes lead to wonderful discoveries. Tom Arnold, owner of Facets Fine Jewelry in Arlington, Virginia, found this out...
Read More
The Ardagh Chalice
Ardagh now is scarcely more than a place-name; it is in County Limerick in Ireland. In 1868, while a peasant...
Read More
The Artists as Curators and Critics
Fortunately, change is inevitable. Even for those individuals in the art establishment who assert that artists cannot and should not...
Read More
The Trouble with Pyrite
The first reference that I have that links copperas with the collection of fossils is found in the 'Life and...
Read More
3 Details of Jewelry Refinement
Quality matters to Michael Bondanza; he has been known to rebuild entire finished pieces -- some containing hundreds of precisely...
Read More
Chemical Inventory and Profiles
If you know what the chemicals are that you use and what their dangers are you will be less likely...
Read More
Basic Approach to Product Design
Design is a perennial issue for all who produce objects meant for a specific use, utilitarian, in contrast to objects...
Read More
Platinum Consideration Factors
Jurgen J Maerz of the Platinum Guild International USA outlines factors to consider when adding platinum to your line of...
Read More
Recycling Gold from Electronics
With over 300 tonnes of gold used in electronics each year, end-of-life electronic equipment offers an important recycling potential for...
Read More
The Ethics of Materials
I have always thought that if no other lesson had begun to seep through peoples' inertia and greed, that at...
Read More
Structuring for Efficiency in the Studio
Being more organized, and planning how you use your time will mean that you will spend less time on some...
Read More
Goldsmithing in the Future
This article is a set of predictions for what the jewelers bench and workshop will experience in technological change in...
Read More
Justifying Art for Art’s Sake
For many years, I have struggled to find ways of conveying the meaning of art and its importance. I had...
Read More
New Generation Gallerists
What does it mean to be a gallerist today, especially one who deals exclusively in art jewelry? To find out,...
Read More
How Jewelers Approach Work Materials
This diagram shows how jewelers approach working in the field in terms of how they relate to the material. The...
Read More
Confidential Disclosure Form
This form may be used if you have an idea for a product and wish to approach a manufacturer. It...
Read More
The Teachers’ Role
I believe the teacher's role is as a guide, an instigator, a devils advocate as well as instructor. A teacher...
Read More
The Digital Tool Debate Continues
In approaching this article, I found there are many avenues to pursue in the exciting and controversial subject of digital...
Read More
The All-In-One Jewelry Making Solution At Your Fingertips
When you join the Ganoksin community, you get the tools you need to take your work to the next level.
Trusted Jewelry Making Information & Techniques
Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.