When sizing rings with stones that may be damaged from heat, hold the stones under water while soldering. To do this, place a metal water cup filled with water on your solder pad. Then support the jewelry with the stones submerged in the water with the place to solder as far out of the water as possible.
To make a water cup, cut the bottom 1″ off a soft drink can. This works particularly well, as the aluminum does not rust as other metal containers do. Fill the cup 3/4 full of fine white sand and cover with water. Then the jewelry you are soldering is easily held in place by sticking the stone down into the sand. In addition, place a small piece of firebrick or cutoff from a ceramic soldering pad through the finger hole of the ring. This helps protect the stones but more importantly, it reflects the heat back up to the bottom of the shank, making soldering much easier.
Paint whiteout over engraving on the inside of rings before sizing or soldering wedding sets together. This will keep the solder from flowing over the engraving.
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.
The All-In-One Jewelry Making Solution At Your Fingertips
When you join the Ganoksin community, you get the tools you need to take your work to the next level.
Trusted Jewelry Making Information & Techniques
Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.