Topaz Gemstone Kinds and Colors


Topaz is a gem that is very often eye clean, so stones with good clarity are available. The red color can be a strawberry hue: these are quite hard to find and will command the highest price. Deep pinks can be exceptionally beautiful. Pink topaz is mined in Pakistan. Pink stones are also available from Brazil; but most of these stones have been heated from orange material. It will not be easy to find the red and deep pink colors; if the color is intense, expect to pay an expensive price per carat. Pastel pinks are also available. These rarer topaz colors generally are found in stones under ten carat sizes.

2 Minute Read

By Sondra FrancisMore from this author
Updated on

The word "topaz" was derived from the sanskit word "tapas" which means "fire". Throughout history, topaz has been used to describe yellow to orange gemstones. Today so much blue topaz is available that some people may think of topaz as a blue gem.

Topaz, 16.09 carats, Brazil
(Photo by ICA/Bart Curren)
Colors:Yellow, orange, pink, blue, brown, colorless and red
R.I.:1.60 - 1.64
Durability:Fragile, has cleavage
S.G.:3.50 - 3.57
Treatment:Irradiation and heating of some colors
Hardness:8
Availability:Some colors abundant, red is very rare
Localities:Brazil, Pakistan, Mexico and Nigeria
Price:Low to expensive
Common shapes:Blues in all shapes; other colors in ovals, cushions and emerald cuts
Topaz, Brazil
(Photo by ICA/Bart Curren)

The most expensive colors of topaz will be the rare red and intense pink colors and some of the very bright orange colors. Fine orange hues of topaz are called Imperial topaz; they may have secondary colors of brown or reds.

(Multi-colored topaz photo by ICA/Bart Curren)

Topaz is a gem that is very often eye clean, so stones with good clarity are available. The red color can be a strawberry hue: these are quite hard to find and will command the highest price. Deep pinks can be exceptionally beautiful. Pink topaz is mined in Pakistan. Pink stones are also available from Brazil; but most of these stones have been heated from orange material. It will not be easy to find the red and deep pink colors; if the color is intense, expect to pay an expensive price per carat. Pastel pinks are also available. These rarer topaz colors generally are found in stones under ten carat sizes.

Imperial topaz colors are easier to find and moderate price per carat prices will be asked for fine quality stones. Brown overtones will lower the value. Pale oranges and golds in smaller sizes may be found in the low price per carat range.

Brown topaz is available but there isn't much demand for it. Some brown topaz has a tendency to fade in sunlight. Brown colors could be a product of irradiation. Smoky quartz is often erroneous called "smoky topaz". Brown shades of topaz will mostly fall into the low price per carat range. Brown and colorless topaz crystals can range is size from small to very large; so any size gem is possible. There is little demand for brown or colorless topaz.

(Various shades of irradiated blue topaz. Photo by ICA/Bart Curren)

Blue topaz is found in nature but it is generally quite pale in color and is rarely available in finished gemstones. Most of the blue topaz found today has been irradiated and heated from colorless or light brown topaz. The color is stable and will not fade. Under extreme heat fading could occur, but it is unlikely you will put your irradiated blue topaz in your self-cleaning oven cycle. Topaz can be treated by various forms of irradiation and a variety of shades occur, which are called sky blue, super blue, London blue, Swiss blue and so on. Blue topaz can be found in almost any size or shape and falls into the low price per carat group.

Topaz is the standard gem for the hardness of 8 on Moh's scale, consequently it is difficult to scratch. But topaz is brittle and has perfect cleavage. The treated stones chip fairly easily. Topaz should be set into protective mountings.

Copyright © Sondra Francis, G.G. 1999
About the Author Sondra Francis has scoured every major colored gemstone market in the world since 1978. She was a charter member of the American Gemstone Association and served as a board member. She was a founding member of the International Colored Gemstone Association. A true gem lover, Sondra has marketed her treasures on the wholesale and retail markets.
________________________________________
Acknowledgments
A special thanks to Pam Dulgar, Alex Edwards, Cheryl Kremkow, Kate Kirby, Helen Mitchell, Carol Morgan Page, David Pond, Elaine Proffitt, and Ray Zajicek for their help.
Photographs: Bart Curren and ICA Gembureau ; Alex Edwards, Pearl Sales Institute ; David Dikinis

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Sondra Francis

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.