Tanzanite Gem Properties
If you are looking at a tanzanite it is critical to view it under different lighting conditions. In daylight tanzanite will display the most blue, incandescent light will bring out the violet color. Generally those stones that are brilliant blue with minimal violet, even in incandescent light, will command the highest price. If you prefer the violetish shades you will pay less.
1 Minute Read
One of the most exciting gem discoveries of the twentieth century is tanzanite, which was first seen in Tanzania in 1967. It was publicized by Tiffany & Co. It has a vibrant blue to blue violet color and can easily be mistaken for the finest sapphire.
| Tanzanite, Tanzania Photo by ICA/Bart Curren | 
If you are looking at a tanzanite it is critical to view it under different lighting conditions. In daylight tanzanite will display the most blue, incandescent light will bring out the violet color. Generally those stones that are brilliant blue with minimal violet, even in incandescent light, will command the highest price. If you prefer the violetish shades you will pay less.
| Colors: | Blue to violet | 
| R.I.: | 1.69 - 1.70 | 
| Durability: | Fragile | 
| S.G.: | 3.20 - 3.40 | 
| Treatment: | Assume heating | 
| Hardness: | 6 - 7 | 
| Availability: | Supply meets demand | 
| Localities: | Tanzania | 
| Price: | Moderate to expensive | 
| Common shapes: | Oval, cushion and fancy shapes available | 
Before the incredible blue shade is created by heat, resulting in tanzanite, the zoisite is a greenish to brownish color which is extremely trichroic. There is some zoisite that has been naturally heated by the sun to turn the material to tanzanite, but most is gently heated before cutting.
| Green chrome zoisite. Photo by ICA/Bart Curren | 
See Also:
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.
The All-In-One Jewelry Making Solution At Your Fingertips
When you join the Ganoksin community, you get the tools you need to take your work to the next level.
Trusted Jewelry Making Information & Techniques
Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.