DIY Metal Shaping Tools: How To Make Your Own Jewelry Hammers Or Mallets


Jewelers spend hours fixing damage that they themselves did to the metal. Soft hammers and shaping tools limit the injuries to the metal being worked, with the best quality of all (the least damage to metal while still shaping it) being paper mallets. Leather however remains tried and true as material for making mallets from.

2 Minute Read

HomeLearning CenterJewelry MakingToolsHomemade ToolsDIY Metal Shaping Tools: How To Make Your Own Jewelry Hammers Or Mallets

Ganoksin may receive customer referral fees from the companies listed in this page.

By Charles Lewton-BrainMore from this author
Updated on

"If you don't want a mark in the metal don't put it there". This simple saying would save jewelers lots of time if they were able to apply them. Jewelers spend hours fixing damage that they themselves did to the metal. Soft hammers and shaping tools limit the injuries to the metal being worked, with the best quality of all (the least damage to metal while still shaping it) being paper mallets.

What You'll Need To Make Soft Hammers and Shaping Tools

As an Amazon Associate, we earn from qualifying purchases referred from our site.

Leather however remains tried and true as material for making mallets from. Some can be found at your local Pet Supply Store.

soft hammers

soft hammers

soft hammers

You can buy round leather dog chews in different diameters at the pet store, cut them in half, drill through them and mount an appropriate sized hammer handle in them to make very inexpensive good quality leather mallets, particularly in the small sizes. Look for one that is solid all the way through as some will have cavities in them. One chew makes about three hammers.

soft hammers

The softer the mallet surface the less damage there is to the metal surface being worked, and the faster it is make a piece. Limiting surface damage is essential for smart goldsmithing.

The Best Soft Hammers & Mallets To Buy

Buy List

Rawhide Mallet

Budget

Garland 11001 Rawhide Mallet, Size-1
Get it on amazon.com
Plastic Mallet

Budget

Plastic Mallet, Size 1, 4 Ounces | HAM-411.00
Get it on amazon.com
As an Amazon Associate, we earn from qualifying purchases referred from our site.

Paper mallets are my favorite because they do not mark the metal at all. Even a leather mallet will damage a metal surface. I know of a pewtersmith who happily spent $400.00 for an old paper mallet - and said it paid for itself in a week. While they aren't produced any more you can make your own: get the widest water based glue packing tape you can, run the tape over a wet sponge and roll it up as tightly as you can, rolling and packing it down until you have a solid roll about 2″ across. Let it dry, drill a hole and insert a hammer handle and you are off to the races

soft hammers

Here is a picture of several soft hammer options, from left to right: a steel hammer with an Aquaplast extension, a paper mallet, a reshaped croquet mallet and a delrin rod to make hammers from.

soft hammers

Horn hammers are pleasant to use and good ones can be made from water buffalo horn (try a knifemaking supplier for sources). Moose and other antlers work but tend to disintegrate in use. An easy place to get a small horn tip to make a hammer with is as an old Horn button for a duffel coat: they come with holes to mount them on a hammer handle.

soft hammers

If you need to shape larger areas of metal. There are wooden knobs from craft stores and furniture components that make good wooden mallets as well as larger sized dapping tools. Here is a selection of knobs.

Originally published under the title: Soft Hammers and Shaping Tools

Ganoksin Staff Note: Finding The Best Types Of Hammers To Use For Your Projects

As discussed above, there are countless types of hammers and mallets used by jewelers at the bench. If you're interested in making some of your own, you can use the materials and techniques listed in this article. You'll also find handy links to the best factory-made mallets above.

Be sure to check out our expert reviews and recommendations of all types of hammers for jewelry work in the Ganoksin Buying Guide. You won't want to miss our helpful insights and up-to-date picks from the leading manufacturers.

All rights reserved internationally. Copyright © Charles Lewton-Brain. Users have permission to download the information and share it as long as no money is made. No commercial use of this information is allowed without permission in writing from Charles Lewton-Brain.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Charles Lewton-Brain

Master goldsmith Charles Lewton-Brain trained, studied and worked in Germany, Canada and the United States to learn the skills he uses. Charles Lewton-Brain is one of the original creators of Ganoksin.

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.