An old lapidary taught me an excellent trick for sealing cracks in gemstones. Some gems are inherently unstable. If a client of mine wants one of these gems for inlay, or to be cut or set, I will often use this technique - with full disclosure, of course - to make the stone suitable for use in these applications. Also, with the growing trend of repurposing old jewelry, I am seeing more sentimental gems coming across my counter that require repair rather than replacement. Enter the epoxy technique.

1 Minute Read

By Gary DawsonMore from this author
Updated on

An old lapidary taught me an excellent trick for sealing cracks in gemstones. Some gems are inherently unstable. If a client of mine wants one of these gems for inlay, or to be cut or set, I will often use this technique - with full disclosure, of course - to make the stone suitable for use in these applications. Also, with the growing trend of repurposing old jewelry, I am seeing more sentimental gems coming across my counter that require repair rather than replacement. Enter the epoxy technique.

To get epoxy deep into a crack in a gemstone, mix it as you normally would and then mix that compound in a 50:50 ratio with acetone. (I generally use water-clear Epoxy 330, which is specifically formulated for use with gemstones.) You can simply paint this new mixture on the crack and it will penetrate very well. As the acetone evaporates, it leaves epoxy in the crack, which cures normally once the acetone is completely evaporated. This curing process may take a few days rather than the normal 24 hours for this particular epoxy, so don't rush it!

To get even better results, immerse the gem in the epoxy-acetone mixture and then place it in a vacuum chamber to boil the mixture, which draws the solution even deeper into the cracks. A formerly unstable gemstone will be ready to set, inlay, or cut after this treatment—and your client will be glad you knew this handy trick.

In association with

The award-winning Journal is published monthly by MJSA, the trade association for professional jewelry makers, designers, and related suppliers. It offers design ideas, fabrication and production techniques, bench tips, business and marketing insights, and trend and technology updates—the information crucial for business success. “More than other publications, MJSA Journal is oriented toward people like me: those trying to earn a living by designing and making jewelry,” says Jim Binnion of James Binnion Metal Arts.

Click here to read our latest articles
Click here to get a FREE four-month trial subscription.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.