Resists and Electroplating to Create Patterns


With the ever-higher cost of precious metals, many jewelers are increasingly working with non-precious metals such as stainless steel, titanium, and copper. As jewelers design with these materials, color and pattern development have become popular ways to dress up the surfaces of these pieces.,,,

3 Minute Read

HomeLearning CenterJewelry MakingSurface ManipulationPatinationResists and Electroplating to Create Patterns
By Charles Lewton-BrainMore from this author
Updated on

With the ever-higher cost of precious metals, many jewelers are increasingly working with non-precious metals such as stainless steel, titanium, and copper. As jewelers design with these materials, color and pattern development have become popular ways to dress up the surfaces of these pieces.

The Prep

An easy way to create colors and patterns on less precious metal surfaces is to use resists and electroplating. Long employed by jewelers in electroplating, resists can be used to block off sections of metal to prevent them from being plated. Several types of resists can be used for creating patterns, including non-conductive paint, electrical tape, nail polish, a thick permanent market, and vinyl sign material that can be computer cut into incredibly detailed geometric patterns.

My favorite resist for this type of project is rubber cement. It should be thinned using rubber cement thinner, which is available at most graphic arts stores. To use, thin down the cement to a watery consistency that you can paint onto the metal. When you are finished plating and are ready to remove it, you can simply rub the cement off the metal with your fingers.

While there are many options available, the plating solutions I use to create colors and patterns are the most standard ones: nickel plating for a gray color, silver plating for white, and gold plating for yellow or gold. Other metal plating solutions, including rose gold, green gold, and rhodium, can be used, all with distinctive colors and brightness.

Additional colors can also be achieved by manipulating the metal after plating. For example, greens and blues can be achieved by rubbing salt water onto a sheet of copper and suspending it in a sealed container with a small amount of ammonia. The ammonia fumes attack the exposed copper (but leave the plating alone), turning it a range of greens and blues. Or the sheet could be heated after plating and then quenched in water: This would turn the exposed copper a range of browns and blacks.

The Process

Before beginning, you must plan out your design for the best results. This process is a bit like painting Easter eggs with a wax resist. Each color is applied one at a time, and earlier colors are protected in parts so that the final result is a piece with lots of colored areas. Your success will depend on how well you planned your design for this technique.

Once your design is finalized, you can begin the plating process, which can be done using a basic rectifier and plating solutions. Take the sheet of metal and apply any texturing you desire. Using your chosen resist, mask off the parts of the base sheet you want left visible, then dip the sheet in the plating solution to add your first color. Five minutes is usually sufficient, but the plating time will vary depending on the desired thickness. Dry the metal's surface and repeat the process, applying resists to any areas you don't want plated with a second color (including the previous plating). Continue this procedure until you achieve the look you desire. Once complete, remove all of the resist material and the multi-colored patterned sheet is ready for use in a jewelry design.

Because these platings are fairly thin, they should be applied to pieces where little to no abrasion will take place, such as earrings, pendants, or brooches, and preferably pieces with raised parts or frames that protect the decorated area from damage. You can also apply a sealer to protect the piece and prevent the colors from changing. I like Nikolas Lacquer, which offers protection from oxidation, perspiration, and abrasion.

In association with

The award-winning Journal is published monthly by MJSA, the trade association for professional jewelry makers, designers, and related suppliers. It offers design ideas, fabrication and production techniques, bench tips, business and marketing insights, and trend and technology updates—the information crucial for business success. “More than other publications, MJSA Journal is oriented toward people like me: those trying to earn a living by designing and making jewelry,” says Jim Binnion of James Binnion Metal Arts.

Click here to read our latest articles
Click here to get a FREE four-month trial subscription.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Charles Lewton-Brain

Master goldsmith Charles Lewton-Brain trained, studied and worked in Germany, Canada and the United States to learn the skills he uses. Charles Lewton-Brain is one of the original creators of Ganoksin.

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.