The Orange Necklace by Chihiro Makio
One of the more difficult challenges Chihiro Makio of 314 Studio in Jamaica Plain, Massachusetts, faced when creating her Orange Necklace was getting the citrus-themed elements to sit properly on the wearers neck. The piece comprises roughly 30 three-dimensional elements, some shaped like oranges and others like leaves, and deciding how to best get them to sit in harmony with one another took some doing.
1 Minute Read
One of the more difficult challenges Chihiro Makio of 314 Studio in Jamaica Plain, Massachusetts, faced when creating her "Orange Necklace" was getting the citrus-themed elements to sit properly on the wearer's neck. The piece comprises roughly 30 three-dimensional elements, some shaped like oranges and others like leaves, and deciding how to best get them to sit in harmony with one another took some doing.
To string together all the odd and sundry shapes, Makio first soldered a bail to the back of each shape. She then cut individual pieces of sterling tubing to fit between each shape, and strung the entire piece together on a sterling neck cord. By cutting each piece of tubing to a length specific to its position, Makio ensured that each element was loose enough to move, but also close enough so that no opening showed between the pieces.
Makio gave the same amount of care to the elements, which were all fabricated from sterling and then surface-treated. She textured the orange pieces by dapping them with a small round tool, then plating them in 24k. "It adds a little more body to it, rather than having a flat circle," Makio says. The leaves have body as well; they are cut from sheet, then cut in half and soldered back together at an angle. A black patina is added for a color contrast to the oranges.
As a finishing touch, Makio decorated the edges of the leaf elements with tiny red and green beads. After drilling small holes in the leaves, she used nylon thread to hand stitch the colored glass seed beads. This final touch took Makio about 20 hours.
But then again, natural beauty does take time.
This piece won first place in the silver category of the 2005 Saul Bell Design Award competition. Photo is courtesy of Rio Grande. |
Bails attached to each element hold the sterling neck cord in place; the cord then passes through sterling tubes between each element. Photo is courtesy of Rio Grande. |
The award-winning Journal is published monthly by MJSA, the trade association for professional jewelry makers, designers, and related suppliers. It offers design ideas, fabrication and production techniques, bench tips, business and marketing insights, and trend and technology updates—the information crucial for business success. “More than other publications, MJSA Journal is oriented toward people like me: those trying to earn a living by designing and making jewelry,” says Jim Binnion of James Binnion Metal Arts.
Click here to read our latest articles
Click here to get a FREE four-month trial subscription.
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.
The All-In-One Jewelry Making Solution At Your Fingertips
When you join the Ganoksin community, you get the tools you need to take your work to the next level.
Trusted Jewelry Making Information & Techniques
Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.