We are a group of artists who call ourselves "Nine Lively Ladies." A year ago, I had to come up with a theme for our 9th show. What better inspiration than our name -Nine Lively Ladies. Each of us would produce 9 pieces, 9 x 9 inches and sell them for $99 - the show would open on the 9th of the 9th month - a good publicity gimmick yes, but a real challenge.

For my pieces, the frame would be 9 inches square using a 6 x 6 inch, thin, white enameled steel that I painted with oxides in oil - one of my favorite techniques. For the sea life pieces, I cut fish shapes from soft rubber to use as stamps while the paint was damp, let it dry thoroughly over night then dry-dumped the powdered enamel with plastic spoon-shaped tools for picking up and dumping the powder. Try practicing letting the dry enamel slide off the side of the tool. This can then be pushed around with a dry brush or pointed wooden tool, then fired one time.

For the pieces where I added fish or silver foil, I had to do a second firing. On some, I cut fish from 26 gauge copper, enameled onto the piece in the first firing. I did whales, dolphins, seahorses, bubble fish with only one firing, and glued magnets to the backs. Same thing with the flower pieces, only painting grassy backgrounds, then dry dumping flower shapes - quite fun! Once fired, butterflies with magnets complete the picture.

One and one half inch squares with letters composed of glass threads, wire or beads on magnets were made for the "Celebrate" piece using a plain 6 x 6 inch steel panel. The letters may be moved around to make many different words… making a game of it.

By Stell Shevis [Volume 28, Number 2, April, 2009]
In association with
glass on metal
Glass on Metal is the only publication dedicated to enameling and related arts. Technical information, book reviews, how-to articles and insight on contemporary enamelers highlight each issue.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Stell Shevis

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.