Modified Setting Bur with Safe Edge Tool


Here iss a nice little tool that makes use of an old setting bur. If you take the bottom teeth off a setting bur and polish the surface, you will have a tool that allows you to get right up next to the wall of a bezel and work on it without harming the metal on the bottom of the piece..

1 Minute Read

HomeLearning CenterJewelry MakingToolsCustomize Your ToolsModified Setting Bur with Safe Edge Tool
By Ronda CoryellMore from this author
Updated on

Modified Setting Bur. Here's a nice little tool that makes use of an old setting bur. If you take the bottom teeth off a setting bur and polish the surface, you will have a tool that allows you to get right up next to the wall of a bezel and work on it without harming the metal on the bottom of the piece.

Take the bur and start grinding or sanding the bottom teeth off. Picture 1.1 shows the use of a belt sander, but a grinder would also work.
Remember to keep a bowl of water handy as you grind to quench the bur so that it does not get too hot, as shown. We don't want to lose the temper of the steel.
Continue grinding until the bottom of the bur is nice and flat as shown above. You should have ground off the entire bottom angled section, and the bottom should be at a 90 degree angle to the teeth on the side walls of the bur.
Once the bur is flat, you will need to polish the surface. As shown in Picture, I used the side of a hard felt wheel on the polishing machine. This allows you to keel the bur perpendicular to the wheel and get a nice uniform surface.
You should see a good reflective surface when you've finished polishing. This Picture shows the single facet on the bur—this is what you're to have when you're finished.
Now you have a tool that will let you get right up next to something you want to work on without worrying about it chewing up the metal underneath. Picture 1.6 demonstrates using this new bur tool right up next to the bezel wall, and the safe edge will protect the bottom of the setting.

Photo by Ronda Coryell and Bill Taroli

 

By Ronda Coryell – © 2004
All rights reserved internationally. Copyright © Ronda Coryell. Users have permission to download the information and share it as long as no money is made-no commercial use of this information is allowed without permission in writing from Ronda Coryell.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Ronda Coryell

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.