Make Your Own Jewelry Displays


Here are some photos of jewelry displays I have made. Bend galvanized sheet metal to make an acute sort of "L" shape, and round the corners a bit with heavy tin snips. Felt will be placed on the front, trimmed to a size just about 5 mm bigger than the metal edges, and then the display will be covered with fabric, in this case a linen-looking cotton in bone white. Fabric with a rough weave or a bit of fuzz is good, so it won't show pin holes in the future when you move jewelry around.

1 Minute Read

By M´lou BrubakerMore from this author
Updated on

Here are some photos of jewelry displays I have made. Bend galvanized sheet metal to make an acute sort of "L" shape, and round the corners a bit with heavy tin snips. Felt will be placed on the front, trimmed to a size just about 5 mm bigger than the metal edges, and then the display will be covered with fabric, in this case a linen-looking cotton in bone white. Fabric with a rough weave or a bit of fuzz is good, so it won't show pin holes in the future when you move jewelry around.

To cover your displays, spray the back of the fabric with spray adhesive, place the felt padding on it, and place the display face down on it. The corners are tricky to do nicely, so I have included a page of instructions. (I learned the corner-covering technique from a bookbinder.) After gluing the fabric cover on, cover the back with felt or paper, and perhaps add stick-on velcro strips to help position chains. Since the felt underlayment is not glued to the board, it can receive U-shaped jewelry pins very well.

These displays, if the feet are all bent at the same angle, stack well for transport. If I want to leave the jewelry fastened to them, I make slipcovers for each one with bubblewrap and tape.

Of course the displays can be made to absolutely any size you like, and can be curved or bent into just the shapes you want. If you want flat displays instead of "L" shaped, you can use corrugated cardboard or mat board as the backing. Look at your transport containers to see how you choose to use that space, before you start making anything.

This system is low-cost, stackable, and easy to make. I like the way it looks, and the fact that I can always recover it with new fabric when it gets shopworn or I just need a color change. I made a large set of it in a day or two.

By M’lou Brubaker – © 2012
All rights reserved internationally. Copyright © ___________. Users have permission to download the information and share it as long as no money is made-no commercial use of this information is allowed without permission in writing from _____________

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


M´lou Brubaker

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.