Please have on hand:

Ear muffs or plugs and safety glasses.

Metal:

  1. Thin copper sheet, 24 gauge (0.5mm) is best, sold often as 'roofing copper'. It is sometimes sold as '16 ounce' copper or .021 copper. Cut into a selection of squares and rectangles for learning.
  2. Aluminum will also work for practicing, again 24 gauge.
  3. Brass wire, 22 gauge, (0.8mm), ten feet or so, round. 18g iron binding wire is also useful.

hammers

Tools:

  • Selection of hammers, mallets and stakes.
  • Raising/forging hammers are most important.
  • A basic T-Stake is very useful.
  • Selection of pliers.
  • Hand shears, aviation snips.
  • Anvil
  • Annealing equipment, soldering equipment and supplies.
  • Access to water for quenching and cleaning. (A kiln can also be used for annealing).
  • Sheet rolling mill and wire rolling mill for rolled folds.
  • Large mounted vise, 6 inches wide or larger. A blacksmith's leg or post vise is also useful.
  • Hydraulic press if available. If so then have on hand some 1/4″ plexiglass scrap for cutting shapes from.
  • Flex shaft, key, silicon carbide separating discs and mandrel for them.
  • Fabulustre® and buff on polishing motor for polishing hammers.
  • A belt sander is very useful for altering forging hammers to improve them.

hammers

hammers
All rights reserved internationally. Copyright © Charles Lewton-Brain. Users have permission to download the information and share it as long as no money is made-no commercial use of this information is allowed without permission in writing from Charles Lewton-Brain.
Buy The Book Japanese Patinas
  • Hardcover: 160 pages
  • Publisher: Brynmorgen Press; 1st edition (April 15, 2008)
  • ISBN-10: 1929565267
  • ISBN-13: 978-1929565269
  • Product Dimensions: 10.7 x 8.3 x 0.7 inches

Purchase your own copy of “Foldforming (Hardcover)” today.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Charles Lewton-Brain

Master goldsmith Charles Lewton-Brain trained, studied and worked in Germany, Canada and the United States to learn the skills he uses. Charles Lewton-Brain is one of the original creators of Ganoksin.

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.