How to Build Up a Thin Shank


This cultured pearl and diamond 14K yellow gold ring is in for sizing. When the take-in person inspected the ring, they noticed that the top portion of the ring shank had worn thin. The shank has become thin and sharp at the top portion. It will be rounded out and built up using an ABI Pulse-Arc-Welder and 14-karat yellow gold 30 gauge round wire. It is not necessary to remove the pearl to do the build up.

2 Minute Read

By Mark B. MannMore from this author
Updated on

This cultured pearl and diamond ring is in for sizing. When the take-in person inspected the ring, they noticed that the top portion of the ring shank had worn thin. The ring is 14-karat yellow gold.

welding thin shank

welding thin shankThe shank has become thin and sharp at the top portion (indicated by arrows). It will be rounded out and built up using an ABI Pulse-Arc-Welder and 14-karat yellow gold 30 gauge round wire.

It is not necessary to remove the pearl to do the build up.

welding thin shankThe pulse-arc-welding pencil contains an electrode (arrow). The electrode is covered by a ceramic collar. Occasionally, the ceramic collar will need cleaning and reshaping. Shown in this image, the inside portion of the ceramic collar for the No. 1 size tip is being cleaned by a diamond tipped bur. (There are 5 different sized tips provided with the ABI Pulse-Arc-Welder.)
welding thin shankThe outside portion of the tip of the ceramic collar is flattened using a diamond wheel. The welding pencil tip is reassembled and placed back in the holding device. The welding pencil is attached to the positive terminal and the alligator clip is attached to the negative terminal.
welding thin shankTo begin building up the shank, the ABI pulse-arc-welder is set for 35 volts on the high energy setting. 14-karat yellow gold 30 gauge round wire is used as a filler material for building up the shank. The round wire is positioned on the edge requiring build up and the ceramic collar on the weld pencil is placed directly over the top. The electrode is recessed about 0.5 millimeters. The energy for welding is discharged by depressing the footpedal. The ABI pulse-arc-welder instantly recharges and the procedure continues until sufficient new metal has been melted to the weak area of the shank.
welding thin shankThe alligator clip is connected to the negative terminal of the welding unit. It is attached to a third hand holding device that's holding the ring for welding. The 30 gauge wire is held directly in the operator's hand. It does not get hot or conduct electricity.
welding thin shankThrough the welding process, excess soot will build up at and near the area being worked. It is easily removed by ultrasonic cleaning. For the best welding adhesion, this soot should be removed as it builds up.
welding thin shankOnce the welding is completed, the ring is again cleaned in the ultrasonic. A rubberized abrasive was used to remove the excess material. All that's left is polishing and cleaning.

Important:

Tack-, fusion- and pulse-arc equipment settings will differ and are based upon the volume, amount of contact and alloy of the material you are working with. Practicing using like materials will give you a parameter for the settings required for your application. Keep a record of settings and tasks for future reference.

By Mark B. Mann Copyright © Mark Mann 2005
Photographs – Mark B. Mann
All rights reserved internationally. Copyright © Mark Mann. Users have permission to download the information and share it as long as no money is made-no commercial use of this information is allowed without permission in writing from Mark Mann.
______________________

This content is published in a handbook along with other welding applications. To get a copy of the ABI Handbook of Welding Applications for Jewelry Design and Repair, contact Janet Kirk at 401-461-4140

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Mark B. Mann

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.