Goshenite – Transparent, Colorless Beryl
Goshenite is the transparent, colorless, alkali-bearing pure beryl that was discovered in Goshen, Hampshire County, Massachusetts. The Lily Pond mine in a pegmatite near a small lake was the source of crystals accompanied by other pale greenish-blue, bluish-green, yellowish, pink, and white beryl crystals.
2 Minute Read
Goshenite is the transparent, colorless, alkali-bearing pure beryl that was discovered in Goshen, Hampshire County, Massachusetts. The Lily Pond mine in a pegmatite near a small lake was the source of crystals accompanied by other pale greenish-blue, bluish-green, yellowish, pink, and white beryl crystals.
Dr. John Sinkankas tells us that originally the designation included "pink beryls" and "pale-colored beryls." The name is now applied to transparent colorless beryls and often includes nearly colorless aquamarine, where the blue tones are undetected. "Lucid" and "white" beryl are terms frequently used by members of the jewelry industry to describe morganite. No trace elements are present in the chemical make-up of goshenite to impart color.
Low dispersion (0.014) may contribute to the infrequent use of goshenite as a desired gem, despite its excellent hardness, toughness, and resistance to corrosive substances. Since the 1st century A.D., the good qualities of colorless beryl have made it an ideal substitute for other colorless gemstones. Silver or green foil is sometimes placed behind the faceted colorless beryl and mounted in a "closed" setting to create imitations of diamonds and emeralds. Doublets and triplets constructed by "sandwiching" sections with colored cement or a thin slice of a synthetic or natural gemstone are used to simulate other valuable gems. The slice of natural gemstone could contain inclusions specific to the imitated gem. Bezel mounts hide the junctures at the girdles of such creations and make the substitution difficult to detect.
Beryl occurs in such quantities of large and often flawless crystals that inclusions in goshenite used for gem purposes are seldom tolerated. Goshenite is found worldwide, but significant deposits lie in various locations in the former U.S.S.R., Mexico, Brazil, and Canada. California, Colorado, Utah, Idaho, South Dakota, North Carolina, Maine, Connecticut, and New Hampshire are all sources of goshenite in the United States.
Gemstone Properties
| Specie | Aquamarine | 
| Composition: | beryllium aluminum silicate Be 3 Al 2 Si 6 O 18 | 
| Class: | silicate; cyclosilicate | 
| Group | beryl | 
| Species: | goshenite | 
| Crystal System: | hexagonal per Arem; hexagonal (trigonal) per Schumann | 
| Variety: | |
| Colors: | colorless | 
| Phenomena: | none | 
| Streak: | white | 
| Diaphaneity: | transparent, translucent to opaque | 
| Habit: | prismatic | 
| Cleavage: | imperfect; none | 
| Fracture: | conchoidal | 
| Fracture Lustre: | vitreous | 
| Lustre: | vitreous | 
| Specific Gravity | varies from 2.60 to 2.90 | 
| Hardness | 7.50 to 8.0 | 
| Toughness: | very good; can be brittle | 
| Refractive Index | o=1.566 to 1.602; e= 1.562 to 1.594 | 
| Birefringence: | varies from 0.004 to 0.008 | 
| Optic Character | uniaxial negative | 
| Dispersion: | 0.014 | 
| Pleochroism | none | 
| Ultraviolet Fluorescence | none | 
| Spectra | not usable | 
| Color Filter | no information | 
| Aqua Filter | no reaction; green indicates nearly colorless aquamarine | 
| Chelsea Filter | no information | 
| Solubility | insoluble in acids except in fluoric acid | 
| Thermal Traits | avoid thermal shock; remove stone during jewelry repairs | 
| Treatments | none | 
| Inclusions | no specific references to inclusions in goshenite were found | 
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.
The All-In-One Jewelry Making Solution At Your Fingertips
When you join the Ganoksin community, you get the tools you need to take your work to the next level.
Trusted Jewelry Making Information & Techniques
Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.