Gabor Forgo


6 Minute Read

By Glass on MetalMore from this author
Updated on

How did you become involved in enameling?

gabor forgo
Observing the World. 21×21 cm. Wall panel, sgrafitto technique. 1991.

This happened accidentally. Having seen some enamel pictures in an exhibition, the quality and intensity of colors highly impressed me and I decided to investigate the technique needed for this art form. So I bought a small booklet to study the means and methods for enameling.

Picture For Meditation. 20×20 cm. Wall panel, sgrafitto technique. 1986.

What is your background and prior work experience?

Expecting Spring. 20×20 cm. Wall panel, sgrafitto technique. 1991.

By profession I have a diploma as an electrical engineer from the Federal Highschool of Technology (ETH) in Zürich with a Ph.D. degree in electrical engineering. I have worked during my whole professional career as a research engineer/manager for office automation. I took early retirement in 2000.

Imaginary Landscape. 10×10 cm. Wall panel, sgrafitto technique. 2002. This is one of a series of 3 pictures, where I tried to create an imaginary landscape by using geometric shapes.

How long have you been involved in enameling?

Butterfly Goblet. 14x14x18 cm. Copper, hand raised butterfly", cloisonné with fine silver. 2003.

I started enameling in 1974 when I bought a small kiln allowing the firing of max. 5 cm x 5 cm large plates. At that time I started to make wall plates combined of this size of squares having subjects from ancient Persian mythologies or flower themes. At the same time I saw a chess set made out of silver which impressed me, although not being a big chess player. Obviously the delicacy of the chessmen and my curiosity, how to produce such fine items, excited my fantasy. So I decided trying to create chessboard and chessmen using enamel on copper.

Blue-Green Goblet. 12×12 cm. Copper, cloisonné with fine silver. 2003.

I made the design for the chessmen out of copper and ordered the appropriate number of truncated copper cones for the soldiers from a local metal workshop. After starting the work I realized the difficulties involved, I took some already finished chessmen and entered a hobby evening course in enameling in Zürich. The teacher judged that my work seemed remarkable and her command of this technology were not much higher than my book-knowledge, nevertheless accepted me as a student and I learned many useful things in these two months.

Dancers. 10x10x20 cm. Copper cut, bent and enameled. 2007. The pieces are glued together after enameling.

What do you find appealing about enameling?

Fortune Key #12. 15×6 cm. 2007. This is a series of 21 "keys", hand sawn out of 1 mm copper plate. The idea for the key was : "We are all looking for happiness, luck and satisfaction. But sometimes, we pass by our luck without noticing it. Had we a key to open the hidden door for luck and happiness, we would see many more smiling faces in the world."

The appeal of enameling for me is twofold : First the quality of colors together with its glass-structure creates a unique finesse enriching any object it is applied to.

The Juggler. 14x14x21 cm. 2008. Copper cut, bent and enameled combined with glass beads.

Second, the element of the fire during processing with all the attendant uncertainties presents challenges to the enameller. This seems to me to be the adventurous part.

Do We Still Have Time? 16×20 cm. Wall panel, sgraffito technique. 2004. This is one picture of a series of five, dealing with the subject " Time". I used poetic quotations of time by Rilke, Proust and others. I tried to create a calligraphic picture.

The numerous different techniques that can be used to reach similar goals allow for individual skills and temperaments. Especially when creating objects, the ease of producing different shapes using copper or other metals is very attractive.

Quarreling. 16×20 cm. Wall panel, sgraffito technique. 1988.

What techniques do you employ when enameling?

Box. 10x10x10 cm. Ceramic box, enameled copper plates. Cloisonné with fine silver. 2003

The majority of my work consists of wall plates on copper with dimensions of max 30 cm x 21 cm as a single plate or larger as a composition of several plates. I mostly use wet painting (Limoges technique). Having a preference for graphic arts with many fine line details, one of my favorites is sgraffito. A further extension of working with lines is the cloisonné technique which I use preferably to decorate objects or for jewelry. I like to combine different materials with different surface structures (shiny and mat, fine and coarse, glass and wood, etc.) using them in a collage-like art. In this way I also overcome the space limits of my kiln to produce larger images. In recent years I started to create abstract objects bending cut copper into different shapes and joining the parts after enameling. I tried to work with acids too, but since there is no water in this room, I did not pursue this path.

Funny Object #1. 22x22x16 cm. Copper cut, bent and enameled combined with glass beads. The pieces are joined together after enameling. 2007.

How does your work evolve? What is the process you employ when creating work in enamel?

Fortune Key #1. 15×6 cm. 2005.

The evolution of my work starts sometimes with a sketch on paper since I like to make line drawings. This I do all the times, having numerous full sketch books by now. I try out the proportions and arrangement of mostly abstract elements on paper before I start sifting the ground layer of enamel. The three dimensional objects are designed ( approximatively ) on paper, but the final shape develops itself during work. Which parts will be joined to which other pieces will be decided in course of the working progress although from the beginning on there exists a definite idea how the finished object should look like. The same applies to the choice of colors.

Joyful. 10x10x20 cm. Copper cut, bent and enameled. The pieces are glued together after enameling. 2007.

How do you develop ideas for your enamel pieces? Do you work from a sketch, or more spontaneously?

Complicated Structure. 16x16x25 cm. Copper cut, bent and enameled. The pieces are glued together after enameling. 2008.

A sketch is an important starting point for the work, but I often use spontaneously an imaginative idea of colors and shapes to create new works. The sketches often provide a preliminary exercise of an idea based on which the final creative process makes its selection whether to use this concept or switch to a completely different concept. In this way, I guess, the spontaneous part is overweighting in my work.

Funny Object #3. 13x13x18 cm. 2007.

Describe your working space…

My workshop is a 25 square meter room in the basement of our house, where my kiln is installed with 5 kW power. 380 V voltage and a horizontal firing chamber of 35 cm x 21 cm x 14 cm (D x W x H). The temperature can be adjusted electronically up to 1100 °C.

Flower Dish. 21×5 cm. Copper, hand raised. Cloisonné with fine silver. 2005.

I have a desk with good light to applicate the colors to the copper plate or object. There is a shelf to store the colors and other useful small items. There is a work table to execute the necessary metal working steps (bending, sawing, hammering, polishing, etc. ) There is no forced ventilation in the room, so I work carefully with sifting or generating dust otherwise.

What inspires your work?

My inspiration is coming from geometry, colors, intricate structures and of course of nature. I do not want to "photograph" pictures, scenes and objects sawn but rather create new artistic objects, express feelings, visualize ideas.

[Volume 27, Number 4, August, 2008]
In association with
glass on metal
Glass on Metal is the only publication dedicated to enameling and related arts. Technical information, book reviews, how-to articles and insight on contemporary enamelers highlight each issue.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Glass on Metal

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.