Cyclosilicate: Axinite


On an excursion in the Alps in 1797, mineralogist, R. J. Hauy discovered some highly vitreous, piezio-electric wedged-shaped crystals that resembled schorl, the dark variety of tourmaline. The incorrect designation, 'vitreous schorl', was used even after axinite was identified as a complicated borate silicate group of minerals. The characteristic axe shape of its crystals gave it its name..

2 Minute Read

By Edna B. AnthonyMore from this author
Updated on

On an excursion in the Alps in 1797, mineralogist, R. J. Hauy discovered some highly vitreous, piezio-electric wedged-shaped crystals that resembled schorl, the dark variety of tourmaline. The incorrect designation, "vitreous schorl", was used even after axinite (Ca,Mn,Fe,Mg)3Al2BSi4O15(OH) was identified as a complicated borate silicate group of minerals. The characteristic axe shape of its crystals gave it its name.

If magnesium is the predominant element of the incorporated ions into its four-member tetrahedral "ring" silicate structure, then it is magnesioaxinite. In ferroaxinite, the iron content is greater than manganese. Manganaxinite is the result if manganese exceeds the iron content. In tinzenite, manganese exceeds the iron content, and calcium is less than 1.5. Since axinite develops in the triclinic crystal system with its low degree of symmetry, and its angles are very acute. Its habit is beautifully illustrated in a picture of rich brown crystals in matrix on page 67 of the Color Treasury of Crystals by Vincenzo De Michele of the Natural History Museum of Milan, Italy.

Massive material in lamellar to granular form is found. Homogeneous growth of the crystals almost always causes feathers and zoning. An excellent photograph of zoning and large two-phase inclusions in a yellow-brown Sri Lankan stone can be found on page 415 of The Photo Atlas of Inclusions in Gemstones by E.J. Gubelin and J. I. Koivula.

Axinite, a metasomatic (replacement) mineral, occurs in contact metamorphic areas in basic rocks and veins. Gem quality material is found in several counties in California, Sri Lanka, and in the French Alps. Deposits of massive material are located in Luning, Nevada, Pennsylvania, and New Jersey. Other sources are Cornwall, England, Finland, Norway, Germany, Japan, Russia, Tasmania, and Mexico. Tinzenite is found in Switzerland and magnesioaxinite in Tanzania.

Crystals large enough to cut gems over ten carats in size are extremely rare. Dr. Joel Arem states in his Color Encyclopedia of Gemstones that "clean stones over 5 carats are —- worthy of museum display". Despite being a bit brittle, its brilliance and sumptuous colors make it a unique and exquisite gemstone.

Gemstone Properties

SpecieAxinite
Composition:(Ca,Mn,Fe,Mg) 3Al2BSi4O15 (OH).
Class:Silicate {Cyclosilicate}.
Group:Axinite.
Species:Magnesioaxinite, Ferroaxinite, Manganaxinite, Tinzenite.
Crystal System:Triclinic.
Varieties:By color, species names & crystallography
Colors:Colorless, yellow, olive green, cinnamon brown, violet brown, pale violet to reddish violet, and blue.
Phenomena:None.
Streak:White.
Diaphaneity:Transparent and translucent
Habit:Distinctive wedge-shape crystals, crystalline aggregate, & massive.
Cleavage:One perfect and some poor.
Fracture:Conchoidal and brittle.
Fracture Lustre:Vitreous.
Lustre:Highly vitreous.
Specific GravityVaries between 3.26 to 3.36; Magnesioaxinite is 3.18
Hardness6.5 to 7.0
Toughness:Fair
Refractive IndexAlpha at 1.674 to 1.693; Beta at 1.681 to 1.701; Gamma at 1.68
Birefringence:0.010 to 0.012
Optic CharacterBiaxial negative; positive if high in magnesium.
Dispersion:High.
PleochroismUsually strong trichroic in reddish-brown, yellow-brown, olive green, yellow, & colorless; In Luning, Nevada material: reddish-brown, deep brown, pale brown, or colorless; In Sri Lankan material: reddish brown, deep violet, & colorless to pale yellow.
Ultraviolet FlourescenceIn Franklin, New Jersey material: SW=red; LW=inert; In magnesioaxinite from Tanzania: SW=dull red; LW=orange-red.
Spectrabroad lines at 4150, 4660, & 4920; narrow line at 5120; possible lines at 4440 & 5320.
Color Filterno information
Solubilitydissolves slowly in HF; use HCl with caution.
Thermal Traitsavoid thermal shock; fusible with intumescence (swelling) at 2.5 to 3.0.
Treatmentsnone known
Inclusionsis seldom flawless; has color zones, feathers, & rare two-phase inclusions.
By Edna B. Anthony, Gemologist P.O.# 62653; Colorado Springs, CO. 80962
All rights reserved internationally. Copyright the New Mexico Faceters Guild © 2002 Users have permission to download this information and share it as long as no money is made. No commercial use of this information is allowed without written permission from the New Mexico Faceters Guild
______________________________
The purpose of the New Mexico Faceters Guild (NMFG) is to bring together persons who are interested in faceting or faceted stones. We promote the art and science of faceting and provide a means of education and improvement in faceting skills. Finally, we provide a means of communication between those persons involved or interested in faceting as a hobby.
______________________________
Meeting Dates: Second Thursday of odd numbered months
Time:     7:00 PM
Place:    New Mexico Museum of Natural History
1801 Mountain Road NW
Albuquerque, NM USA

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Edna B. Anthony

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.