This article by Steve Satow shares a step by step procedure on how t o make a customized ultrasonic sediment bucket.

image_1

These are the parts you need for this project: A Gilmore plastic ball valve (that unlike regularball valves doesn't choke down at the valve as it stays a full 1/2 inch wide for faster gravity fed drainage), O-rings, silicone grease, and a 1/2 inch PVC fitting for a threaded outdoor electrical box and a piece of scrap black vinyl screen door material.

image_2

An old empty kitty litter pail as square pails waste less space and the gasket seals better with flat sides.

image_3

Measure to the center of the bucket, then up 3Vz inches up from the bottom. Then make a mark for drilling.

image_4

Measure the PVC electrical fitting and drill out a hole to fit the OD of the threaded end.

image_5

Take the PVC fitting and make sure the hole is the right size and has no rough edges.

image_6

Take out one of the gaskets and roll it over the threaded portion of the PVC fitting. It should fit tightly against the fittings shoulder.

image_7

After fitting the gasket, apply a heavy layer of silicone grease on both sides.

image_8

Screw the PVC fitting through the side of the bucket until its snug. Then screw the ball valve on to the other side until it's very tight.

image_9

Screw the ball valve onto the other side until it's very tight.

image_10

The ball valve is now ready to quickly drain the ultra bucket after all the precious metals dust has settled to the bottom.

image_11

Cut out the inside of the bucket lid.

image_12

Cut a piece ofthe vinyl screen to fit the bucket like this.

image_13

Snap the lid over the screen material so you have a replaceable filter to catch melee and other small parts that fall to the bottom of the ultrasonic. Trim the vinyl back to the edge of the lid with household shears as in the picture.

By Steve Satow – © Bench Magazine
In association with
BENCH Magazine is devoted to the Bench Jeweler in retail jewelry stores and small trade shops.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.