Customized Turntable Tool Rack


3 Minute Read

By Steve SatowMore from this author
Updated on

Find a turntable that
 is size appropriate for 
your bench. In this case
mine is 18 inches wide.
 If possible find one with 
ball bearings to make it 
work smoother. Buy a 1/4
 sheet of sanded on one
 side 1/2 inch plywood
 and a 3 foot piece of 
5/8 inch wooden dowel. 
(Other supports can be
used for risers. I have used 1/4 in threaded rod. )

image_1

Lay the turntable on the plywood base you purchased. Trace around the base and use a saw to cut it out. Sand the edges to remove all burs.

image_2

Cut your risers to whatever height you can reach comfortably while seated at your bench or whatever height you need for what you will be storing on your bottom shelf. Decide what distance works best for you with what you're storing on the bottom of the unit and for how far from the edges you want it spaced.

image_3

Lay the base on top of the plywood piece you cut out and drill through both at once so they line up. Pre-drill the risers so the riser won't split when you put in the screws. Use 1 5/8 inch dry wall screws. I set mine in about 4 inches from the edge and made them about 9 inches tall. I went 9 inches tall because I have some long plier handles and I didn't want them to block the lower shelf.

image_4

The flexible steel track for the edge is scrap strapping that Home Depot uses to hold bundles of wood together. You can usually find some for free at lumber suppliers. Purchase at the hard- ware store 2 packs of 1 inch corner braces a
package of l0 - 1/2 inch
sheet metal screws, a package of 10 -11/2 inch 10-32 machine screws and a 100 pack of washers to fit the 10-32 screws.

image_5

I flipped my plywood top here and put in two screws to hold it until I finished installing the plier holding steel band. Depending on the size of your turntable lay out how many braces you think you will need. I used eight of them. Lay the corner braces as pictured to the edge of the plywood and mark the place to pre-drill the screw holes. Install the 10-32 screws with 15 washers as pictured to space it out I inch. Then drill a hole to fit the 10-32 screw in the end of the steel strapping and install one end.

Now trying to keep your spacing even, wrap the strapping around to each corner bracket with the 1 inch of washers already installed. Mark with a magic marker where the screw head hits and drill them one at a time as you work your way around. This is the easiest way to make them even.

image_6

Here you see the finished top ready to be unscrewed from the risers and ready to be flipped over.

image_7

This is a close up of how far the steel strip should be placed from the top after it is flipped. This spacing works with most pliers. If it needs to be lower, take the top off again and place an even amount of wide fender washers under the corner braces to lower them from the wood once it is flipped over again.

image_8

This is the rack all 
ready to paint. I also 
put carpet on top of 
mine so heavy bench mate products would 
not chip the paint. I 
hope you enjoy your
 new tool rack. For a
 quick reference on the 
pliers you use all the
 time add plastic clothes
 hangers of different colors and put the pliers that you use for different jobs between them. As you spin the unit around they all blend together but with clips of different colors they stand out.

By Steve Satow – © Bench Magazine
In association with
BENCH Magazine is devoted to the Bench Jeweler in retail jewelry stores and small trade shops.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.