With these pliers you can pre polish platinum and gold peg heads of any shape. Remove any nicks one prong at a time at your bench with a pumice wheel then off to the polisher and right into the sonic, them steamed all while clamped in the same plier.

Customized Loose Head Holder Procedure

image_1These pliers are made with an in- expensive pair of long nose pliers
image_2Use a separating disk to make short work of cutting down the pliers. Make one side slightly shorter than the other (wear safety glasses)
image_3Gently round the corners after cut- ting off the ends to remove burs.
image_4Cut deep notch with the separating disk in end of the shorter plier tip.
image_5Use a #2D finishing nail and round the end slightly. Then, Laser weld the nail to the short end that you notched. Torch solder it on if a laser isn't available. Cut off the excess with a separating disc.
image_6Cut a deep notch into the other tip with a 2 mm ball bur.
image_7Bend the tip till if is centered perfectly in the hole. If you have to torch solder it into place be sure to temper it again after you solder it on.
image_8Now you're ready to take out the deep nicks with a pumice wheel.
image_9Polish the head now with the peg facing up, do one prong at a time. Rotate it with your fingernail till they are all done. Then swish it in the ultra-sonic and steam it off ready to solder in place.
By Steve Satow – © Bench Magazine
In association with
BENCH Magazine is devoted to the Bench Jeweler in retail jewelry stores and small trade shops.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.