A worn-out bristle brush can easily be recycled into a useful tool called a whip burnisher or rotary hammer to improve or even eliminate minor imperfections and surface porosity in castings and other metal surfaces.

1 Minute Read

Updated on

A worn-out bristle brush can easily be recycled into a useful tool called a whip burnisher or rotary hammer to improve or even eliminate minor imperfections and surface porosity in castings and other metal surfaces.

You'll need the following supplies, which are available at most jewelry shops, to make a whip burnisher:
  • worn-out bristle brush wheel
  • flex-shaft and handpiece
  • bench grinder with a coarse grit wheel and a medium grit wheel (such as a cratex wheel)
  • jeweler's saw
  • sanding sticks - 320, 400 and 600 grit
  • polishing machine with tripoli and rouge buffing wheels

The first step is to use the jeweler's saw to cut off the worn-out bristle brush. This will leave just the shaft of the former brush wheel — a piece of mild "soft" steel about an inch and a half long. This type of steel works well because it's not hardened or tempered. It's strong, but you can still bend it easily without breaking it.

Use the coarse grinding wheel on the bench grinder to round the end steel piece. Remove coarse grinding marks with the medium wheel, then insert the steel into the flex-shaft handpiece and spin it against 320, 400 and then 600 grit sandpaper sticks to make a smooth, rounded end. Finally, polish the rounded end with tripoli and rouge.

The last step is to make a slight bend about 6-7 mm from the end you have rounded and polished. The further you bend the stock, the more aggressive the burnisher will be when you use it. You can adjust the tool to suit your preferences as you use it.

To use the whip burnisher, insert it in the flex-shaft handpiece and spin it at medium speed. Bring a metal surface against the spinning end, and it will hammer the surface and smooth out imperfections, such as porosity. A touch of burr lubricant will improve the performance of the whip burnisher.

Lightly sand the surface of your piece with 400 and 600 grit sandpaper after burnishing it, then polish as usual.

Watch The Video:

By Don Hughes – © GIA – 2011
In association with
Art Jewelry
For more information on GIA‘s Jewelry Manufacturing Arts program, click here.
All rights reserved internationally. Copyright © GIA. Users have permission to download the information and share it as long as no money is made. No commercial use of this information is allowed without permission in writing from GIA

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.