My formal education includes a Bachelors Degree in Chemical Engineering and a Masters Degree in Mechanical Engineering. My interest in enameling started when my son received an enameling kit as a present. I was intrigued with the beauty and permanence of the enamels on metal surfaces. Upon retiring from my engineering position with the Department of Defense in the Pentagon, I decided to actively pursue the making of enamel jewelry as a hobby. To further this goal. I took numerous courses in all phases of enameling at Montgomery College in Rockville, Maryland and this was supplemented by attending workshops given by world-class enamelists. In addition I attended college level courses at the University of Maryland.
After experimenting with the various techniques of enameling I decided that champlevé jewelry best suited my interest. Being very familiar with the usual etching methods of scoring the metal, I thought the process was rather cumbersome and in some instances lacking in precision. As an engineer I was familiar with the machining of metals and acquired a small milling machine to score the metal for champlevé enameling.
The Milling Machine
Figure A shows a picture of a small milling machine suitable for mounting on a worktable. Basically, the machine can be considered a sophisticated drill press utilizing bits called end mills. These bits have a flat bottom so that the cut is smooth.
The machine shown in the exhibit [there are others] consists of two parts: 1) a vertical milling head about 23 inches high weighing about 16 pounds and, 2) a milling table about 19 inches long and 4 inches wide weighing about 30 pounds. The unit is shown with an accessory to permit precise angular and circular scoring of the metal.
The particular feature which distinguishes the milling machine is the precise control of the milling bit [to .001 inch] in the X, Y, and Z directions by means of turning 2 wheels and a screw which regulates the depth of cut. The milling bits are available in many sizes permitting the width of cut or diameter of a hole to be precisely controlled.
Making a Champlevé Jewelry
As with all jewelry, the first step is to develop a design utilizing the capabilities [and limitations] of the milling machine and the application of enamels. Based on experience, the best metal thickness for enameling utilizing the milling machine is 16 gauge in fine silver or copper. In view of the precise control needed in the depth of cut the metal must be absolutely flat. The optimum depth of cut is normally one half the thickness of the metal. The blank metal piece is secured firmly to the table of the machine which is precisely moved under the rotating milling bit by turning the control wheels and depth screw. Normally it is necessary to make several passes of the milling bit to reach the final depth of cut. The scored metal is removed from the machine and normal enameling procedures utilized to make the finished piece of jewelry.
The pictures shown illustrate the versatility of the milling process in producing precise crisp cuts for application of enamels. The jewelry produced should provide an interplay of lines and planes in geometric patterns coupled with the shading and luminosity of the enamels chosen for the individual design. To my knowledge I am the only enamelist utilizing this technique for making champlevé jewelry.
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.
The All-In-One Jewelry Making Solution At Your Fingertips
When you join the Ganoksin community, you get the tools you need to take your work to the next level.
Trusted Jewelry Making Information & Techniques
Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.