A ring roller designed to enlarge rings can be used to tighten stones in a channel set wedding band. Select a half-round die larger than the width of the band; making certain the die will contact the tops of the channel without hitting the stones.

image_1image_2

Apply gentle pressure and roll across the entire channel, compressing the metal down tight onto the stones. Then, remove the ring and check the stones. Repeat as necessary. DO NOT Over Tighten The Die Against The Ring. This process will leave the channel smooth and even.

~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

If you're tired of butterfly guards breaking, pinching or snagging or the sticker shock of other arthritic shanks try this idea. It has worked for over a year on this Platinum ring. order 18Kw gold to make it. I used 1 x .75mrn flat shank material and rolled it to .5mm to add spring. The metal is then curved to match shank shape. Make a jump ring that is proportioned like picture and solder it on to end.

image_3

Curve the jump ring so when the pieces spring down toward the shank they give each other stability as well as not pinching the skin. This also makes the jump ring act like a guide. Make sure when fully compressed against the shank that the jump ring side still overlaps slightly. Solder the non jump ring side first so aligning the jump ring side with the correct amount of flex is easier to do.

- Steve Satow (see article for Tools Alterations)

~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

image_4
Ball of Jett Sett in use in a bench mate.

Take a warm ball of Jett Sett and squeeze the lower third in a ring clamp. Then, allow to cool.

image_5
Backside of Jett Sett ball.

To use re-heat the top of the ball to secure the item of jewelry and re-clamp the ball in your ring clamp.

~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

See Also:
In association with
BENCH Magazine is devoted to the Bench Jeweler in retail jewelry stores and small trade shops.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Bench Magazine

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.