Laser Repair: Bangle Bracelet


1 Minute Read

Updated on

It's an "everyday" kind of repair job. The customer brings in a bangle bracelet that has a broken safety slide. This time let's try a different approach to repairing it. After a close inspection of the bracelet we have determined that he safety slide has broken off inside the bracelet.

image_1

In the past I would take off the end cap of the bracelet, "fish-out" the broken bar, replace the end cap (CAREFULLY), solder it in place, reattach the bar to the clasp tongue, and then reinsert the end of the slide bar into the bangle. Start to finish, probably a 15 to 20 minute job (including clean up).

image_2

This time, using the laser, we will complete the job in 5-7 minutes with very little clean up.

Here's how to do a Bangle Bracelet Repair

Drill a hole into the top of the bangle bracelet about 5mm back from the end cap. The the end cap of the bracelet on the edge of your work bench to move the broken slide toward the end cap.

image_3

Insert a small pointed instrument (I used a small screw driver), into the hole and with a down and forward motion, push the broken piece through the end cap slit opening and outside the bangle. Pull out the rest of the slide with a pair of pliers, solder it to the clasp tongue and reinsert the repaired slide back into the bangle.

image_4image_5

Now it's time to plug the hole. Use a gauge wire that fits tightly into the hole and insert it just enough to plug the hole. Be careful not to inset the wire too deeply so it doesn't hinder the movement of the slide inside the bangle. Laser weld around the perimeter of the wire where it touches the top of the bangle.

image_6

Clip off the excess wire, file, and polish.

This makes a tedious repair a fast and enjoyable one! Give it a try; I think you'll like it!

By Bob Staley – © Bench Magazine 2004 Fall
In association with
BENCH Magazine is devoted to the Bench Jeweler in retail jewelry stores and small trade shops.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.