Additive Manufacturing in the Jewelry Scene
Did you ever imagine you'd see the day when a finely woven mesh bracelet with thousands of tiny links could be grown in one piece, on a machine, using 18k gold powder? Well, that day has come. It's jaw-dropping, really.
5 Minute Read
Today, thanks to additive manufacturing, an intricate piece of jewelry something that used to take countless days of hand labor to make can now be produced overnight on a laser melting machine. The machine builds up a net shape, layer by layer, much the same way as a rapid prototyping system does only instead of resin materials, the layers are made of metal powder.
Did you ever imagine you'd see the day when a finely woven mesh bracelet with thousands of tiny links could be grown in one piece, on a machine, using 18k gold powder? Well, that day has come.
It's jaw-dropping, really.
The manufacturing technology itself isn't all that new it's been in use for more than a decade in other industries, such as medical, dental, aerospace, and automotive. What's new is how it's been adapted for jewelry making, which has its own unique demands. Those other industries don't work in precious metals, nor do they require pristine surface finishes: You can take a belt sander to a large steel auto part to smooth it out, and any metal loss is financially insignificant. You can't say the same for an 18k gold pendant.
For years, the technology couldn't make that leap and produce high quality "builds" with good surface finishes: the powders weren't good enough, nor were the laser melting machines small enough to accommodate jewelry making. Now, thanks to smaller machines and, most important, recent developments in precious metal powders, it can.
"The trick to powder metal technology is in making and selling the powder, not the machines," says Steven Adler of A3DM Technologies in Portland, Oregon, a member of MJSA's Thinking Ahead Advisory Council. "There are a number of machines on the market that would be able to grow jewelry pieces from precious metal powder, but there are only a handful of powder suppliers at present." And those suppliers have been working hard to atomize various alloys of precious metal powder to achieve the particle sizes necessary to obtain the fine surface finish required in jewelry production. At presstime, precious metal powder was available in gold and silver only, not palladium or platinum, from four suppliers: Cookson Precious Metals, Hilderbrand, Legor, and Progold.
A New Option
It's important to point out that companies heavily invested in additive manufacturing technology don't view it as a replacement for the lost — wax casting process, but rather as an additional option in the jewelry manufacturer's repertoire.
"The real potential for this technology is in designs that are difficult or impossible to make using traditional casting techniques," says Brian Romanoff of Romanoff International Supply Corp. in Amityville, New York, the U.S. distributor of the Mlab laser melting machine by Concept Laser. Romanoff points to link chain as an example of a jewelry item especially suited to this process. "Instead of casting components separately and then soldering or laser welding them to arrive at the finished piece, you can eliminate countless labor hours by growing the pieces from powder," he says. "This was never before possible in the jewelry industry."
David Fletcher, Euro — pean product manager for Cookson Precious Metals in Birmingham, England, likewise sees the biggest opportunities for laser melting in complex designs. "This technology really stands out when it's used to produce parts that can't be made any other way, such as mesh and hollow forms," says Fletcher. "If a standard jewelry item such as a wedding ring or band can be manufactured successfully with lost — wax casting, it's probably more cost — effective to keep making it that way."
Since it partnered with laser melting machine manufacturer EOS 15 months ago, Cookson has been traveling to jewelry shows and conferences worldwide to educate manufacturers about the technology. The company offers a total manufacturing solution, including 18k gold powder (with other powders in development), the laser melting machine, and technical support, as well as a service bureau for designers.
Industry Response
While the potential is obvious, the response to this new technology among jewelry industry veterans has so far been mixed, with most citing cost as the biggest roadblock to implementation. The average investment in a laser melting machine suitable for jewelry production ranges anywhere between about $160,000 and $300,000before you account for the powder needed to operate it.
"If you are considering even one of the smallest laser melting machines available for 18k gold, factor in a little over $100,000 for the 2 kg of gold you need to operate it," says Linus Drogs of Au Enterprises in Berkley, Michigan, a member of MJSA's Thinking Ahead Advisory Council. "The technology is a fabulous advance for our industry, but it's only realistic for a very few companies with deep pockets to use it for precious metal powder."
J. Tyler Teague of JETT Research in Johnson City, Tennessee, who is also a member of the Thinking Ahead Advisory Council, sees limited application in the marketplace at this time. "Jewelry manufacturers who make jewelry for royalty could probably afford to implement this technology," he says. "If you make very high end, complex custom orders a few pieces at a time, this could work for you."
Drogs and Teague agree that if the build envelope for these systems could be minimized, thus requiring less powder to operate, the technology would be a more viable option for gold jewelry manufacturing in the current metals market. "If you could scale down the build chamber and pop out one piece at a time using only 0.25 kg of gold, the technology would be more widely applicable," says Drogs.
For those who want to test out the technology without making a large financial investment, both Cookson and Legor currently offer a service bureau option, in which jewelry designers or manufacturers pay a feeas they do to a contract caster — to submit CAD files to be grown on a laser melting system. Because the biggest potential for this manufacturing process now is building pieces that are difficult or impossible to cast, it would seem to offer wide appeal to designers and custom jewelers who love dreaming up wild creations for which production is limited by the boundaries of the lost — wax casting process.
The potential for this cutting — edge technology to unleash creative freedom in the jewelry industry is exciting, and designers and manufacturers have only just scratched the surface of what is possible when imagination and technology come together. Stay tuned.
The award-winning Journal is published monthly by MJSA, the trade association for professional jewelry makers, designers, and related suppliers. It offers design ideas, fabrication and production techniques, bench tips, business and marketing insights, and trend and technology updates—the information crucial for business success. “More than other publications, MJSA Journal is oriented toward people like me: those trying to earn a living by designing and making jewelry,” says Jim Binnion of James Binnion Metal Arts.
Click here to read our latest articles
Click here to get a FREE four-month trial subscription.
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.
The All-In-One Jewelry Making Solution At Your Fingertips
When you join the Ganoksin community, you get the tools you need to take your work to the next level.
Trusted Jewelry Making Information & Techniques
Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.